PROPRIETARY SIHARD 2833 Tool steels
Data updates
This material has 30 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY SIHARD 2833 Chemical Composition
SIJ Metal Ravne, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY SIHARD 2833 Physical Properties
Temperature
This material has 30 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY SIHARD 2833 Heat Treatments
- Soft annealing: Heat to 680-720°C, cool slowly. This will produce a maximum Brinell hardness of 213.
Stress relieving: Stress relieving to remove machining stresses should be carried out by heating to approx. 600-650°C, holding for 1-2 hours at heat, followed by air cooling. This operation is performed to reduce distortion during heat treatment.
Hardening: Harden from a temperature of 760-800°C followed by water quenching. Hardness after quenching is 65 HRC.
Tempering temperature: 100-200°C.
PROPRIETARY SIHARD 2833 International Equivalent Materials
Showing 6 of 10 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 10 international equivalents?
See all 10 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 10Cross References
- 4Composition
- -Mechanical Properties
- 9Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 6Total Suppliers