GS-60.3 (Germany / TGL) Material Properties

Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / TGL

Data updates

Latest Update: 2021-01
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 600 MPa view details
Elongation, A 15 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Strength 250 kJ/m² view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 87 ksi view details
Elongation, A 15 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Strength 119 ft·lb/in² view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.40 – 0.50
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

TGL 14 315/01: 1985 / Unalloyed Steel Castings; Types

Heat Treatments

  • Normalizing: 840 - 870°C; Stress relief annealing: 550 - 650°C.