DTD 5072 Cast steels
Data updates
This material has 77 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DTD 5072 Chemical Composition
D.T.D. 5072: 1958 / 75 - 85 Ton Steel Investment Castings - Non-Stainless
Looking for full material performance data?
Free registration required • Instant access
DTD 5072 Heat Treatments
- All castings shall be normalized or annealed by heating at a suitable temperature within the austenitic range.
No casting shall be hardened more than three times.
DTD 5072 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DTD 5072 International Equivalent Materials
Showing 4 of 68 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 68 international equivalents?
See all 68 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 68Cross References
- 2Composition
- 6Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers