GS-45 Mn 4 (Germany / TGL) Material Properties

Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / TGL

Data updates

Latest Update: 2020-07
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 590 MPa view details
Elongation, A 10 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Strength 300 kJ/m² view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 590 MPa view details
Elongation, A 10 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Strength 300 kJ/m² view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.40 – 0.50
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

TGL 14 395/01: 1985 / Low-alloyed Steel Castings; Types

Heat Treatments

  • Normalized: 830 - 880°C<br>Hardened: 820 - 860°C cooled in water or oil<br>Tempered: 530 - 670°C<br>Stress relived: 550 - 650°C<br>The temperature of the stress relieving annealed must be cooled down to about 250°C