FLC-4608-75HT (United States / MPIF) Material Properties

Material group: Ferrous Alloys / Sintered powdered metals
Country/Standard: United States / MPIF

Data updates

Latest Update: 2021-03
Total number of updates: 2
Update History:
2020-02

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Compression Yield Strength val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 520 MPa view details
Elongation, A ≤ 1 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Rockwell Hardness (HR) 32 view details
Compression Yield Strength val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 75.4 ksi view details
Elongation, A ≤ 1 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Rockwell Hardness (HR) 32 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 130 GPa view details
Density 6.7 — 6.8 kg/dm³ view details
Poisson Coefficient 0.27 view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Modulus of Elasticity 18.9 E+03 ksi view details
Density 0.242 — 0.246 lb/in³ view details
Poisson Coefficient 0.27 view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.6 – 0.9
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cu
VALUE
1.0 – 3.0
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
Balance
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Other
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER

MPIF Standard 35 - SP: 2024 / Materials Standards for PM Structural Parts

Heat Treatments

  • Tempering temperature for heat-treated (HT) materials: 180°C (350°F).