AISI D6AC Structural and constructional steels
Data updates
This material has 59 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AISI D6AC Physical Properties
Temperature
This material has 59 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AISI D6AC Heat Treatments
- Normalizing: 927-954°C (1700-1750°F), air quenched. Annealing: 829-857°C (1525-1575°F). Furnace cool to 538°C (1000°F) or below (rate of furnace cool should be 28°C (50°F) per hour or slower). Recommended subcritical anneal temperature is 677°C (1250°F).
Austenitizing: 913-941°C (1675-1725°F). Medium for quenching: oil.
AISI D6AC Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AISI D6AC International Equivalent Materials
Showing 7 of 7 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 7 international equivalents?
See all 7 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 7Cross References
- -Composition
- 4Mechanical Properties
- 19Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 2Fatigue
- 22Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 3Total Suppliers