S500MLHCO (European Union / EN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: European Union / EN

Data updates

Latest Update: 2022-08
Total number of updates: 3
Update History:
2022-04 2019-08

Mechanical Properties


Temperature

≤ 0°C
0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 480 MPa view details
Tensile Strength 580 — 760 MPa view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 69.6 ksi view details
Tensile Strength 84.1 — 110.2 ksi view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
0.015 – 0.055
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
As
VALUE
≤ 0.03
UNIT
%
CAS NUMBER
7440-38-2
CRITERIA
B
VALUE
≤ 0.0008
UNIT
%
CAS NUMBER
7440-42-8
CRITERIA
Bi
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-69-9
CRITERIA
C
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
C+Nb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Ca
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-70-2
CRITERIA
CEV
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Cr
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Nb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
Nb+Ti+V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Nb+V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
Pb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Pcm
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Sb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-36-0
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Sn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-31-5
CRITERIA
Ti
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2

EN 10225-4: 2019 / Weldable structural steels for fixed offshore structures - Technical delivery conditions - Part 4: Cold formed welded hollow sections

Heat Treatments

  • After welding, test welds which are to be tested in the PWHT condition shall be post-weld heat treated at either 580°C ± 20°C or at another temperature to be agreed by the purchaser and the manufacturer. They shall be subjected to a soaking period of either not less than 1h per 25 mm wall thickness or 4h, whichever is the greater. Heating and cooling rates shall be in accordance with the following: <br> The rate of heating shall not exceed (5 500/T)°C/h or 55°C/h, whichever is the greater, where T is the wall thickness in mm.<br> Test welds shall be cooled to a temperature of 400°C at a rate not exceeding (6 875/T)°C/h or 55°C/h, whichever is the greater.