TCVN X2CrCuTi18 Stainless steels
Data updates
This material has 32 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TCVN X2CrCuTi18 Chemical Composition
TCVN 10356: 2014 / Stainless steels − Chemical composition
Looking for full material performance data?
Free registration required • Instant access
TCVN X2CrCuTi18 Physical Properties
Temperature
This material has 32 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TCVN X2CrCuTi18 Heat Treatments
- Hot forming: heated at 1100-800°C, cooled in air; Annealing: heated at 800-1050°C, quenched in water or cooled in air.
TCVN X2CrCuTi18 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TCVN X2CrCuTi18 International Equivalent Materials
Showing 3 of 5 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 5 international equivalents?
See all 5 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 5Cross References
- 18Composition
- 3Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers