TCVN X12Cr13 Stainless steels
Data updates
This material has 726 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TCVN X12Cr13 Chemical Composition
TCVN 12142-18: 2017 / Heat-treatable steels, alloy steels and free-cutting steels - part 18: Bright Steel Products
Looking for full material performance data?
Free registration required • Instant access
TCVN X12Cr13 Physical Properties
Temperature
This material has 726 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TCVN X12Cr13 Heat Treatments
- Hot forming: heated at 1100-800°C, cooled in air; Annealing: heated at 750-810°C; Quenching: heated at 950-1010°C, quenched in oil or cooled in air; Tempering: heated at 700-780°C (+QT1) or heated at 620-700°C (+QT2).
TCVN X12Cr13 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TCVN X12Cr13 International Equivalent Materials
Showing 15 of 401 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 401 international equivalents?
See all 401 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 401Cross References
- 21Composition
- 47Mechanical Properties
- 4Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 252Total Suppliers