PROPRIETARY Kobalt 3 Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2021-01
Total number of updates: 2
Update History
2019-05

This material has 13 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Kobalt 3 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.81
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Co
VALUE
2.6
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Cr
VALUE
4.2
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-33-7

Edelstahlwerk W. Ossenberg & Cie. GmbH, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Kobalt 3 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 13 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Kobalt 3 Heat Treatments


  • Hot forming and heat treatment: Forging at 1120 - 900°C; Annealing at 850°C for 8 h.
    Hardening (quenching in oil, air or hot bath): 1240 - 1270°C.
    Tempering temperature: minimum 540 - 560°C, 2 x 1 h.

PROPRIETARY Kobalt 3 Mechanical Properties


Temperature

PROPERTY / VALUE
Brinell Hardness (HB)
≤ 300
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
63 — 65
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 6Composition
  • 2Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers