PROPRIETARY Ultra 254 SMO Stainless steels
Data updates
This material has 235 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY Ultra 254 SMO Chemical Composition
Outokumpu, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY Ultra 254 SMO Physical Properties
Temperature
This material has 235 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY Ultra 254 SMO Heat Treatments
- Hot forming at 1200-1000°C.
Solution annealing at 1150-1200°C.
Quenching with water at a thickness above 2 mm, below 2 mm an annealing temperature of 1120-1150°C and cooling with air/water can be used.
PROPRIETARY Ultra 254 SMO Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY Ultra 254 SMO International Equivalent Materials
Showing 15 of 128 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 128 international equivalents?
See all 128 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 128Cross References
- 6Composition
- 27Mechanical Properties
- 10Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 3Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 3Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 57Total Suppliers