SAE NC310YW Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country / Standard: United States / SAE

Data updates

Latest Update: 2019-12
Total number of updates: 2
Update History
2019-01

This material has 6 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

SAE NC310YW Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 6 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

SAE NC310YW Heat Treatments


  • Annealing by heating to 920 ± 14°C (1688 ± 25°F) for 1 hour, cool to 700 ± 14°C (1292 ± 25°F) and maintain at 700 ± 14°C (1292 ± 25°F) for 24 hours. Normalizing temperature: 975°C (1787°F). Normalizing temperature can be set between 950 - 990°C (1742 - 1814°F). Austenitizing temperature: 940°C (1724°F).
    Austenitizing temperature can be set between 910 - 950°C (1670 - 1742°F). Sub-zero no more than -70°C (-94°F) is required for obtaining maximum hardness. Hardening quenchant: oil, polymer, inert gas.
    Tempering: 300°C (572°F), at least two tempering operations are required.
    All parts, shall be in one of the following conditions prior to austenitizing: normalized, normalized or tempered or hardened. If those parts have been normalized only without tempering or overaging, they shall be preheated before exposure to the austenitizing temperature.

SAE NC310YW Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1931 — 2103 MPa
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
53 — 56
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • -Composition
  • 2Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers