SEW 22NiMoCr37 Structural and constructional steels
Data updates
This material has 91 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SEW 22NiMoCr37 Chemical Composition
SEW 640: 1975 / Steels for components in the primary circuit of nuclear power plants
Looking for full material performance data?
Free registration required • Instant access
SEW 22NiMoCr37 Physical Properties
Temperature
This material has 91 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SEW 22NiMoCr37 Heat Treatments
- Hardened at 880-940°C, cooled in air or quenched in oil or water
Tempered at 600-700°C
Stress relief annealed at 550-620°C. This temperature should be at least 30°C below the tempering temperature and should not exceed the upper limit of the temperature range indicated
SEW 22NiMoCr37 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SEW 22NiMoCr37 International Equivalent Materials
Showing 1 of 1 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1 international equivalents?
See all 1 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1Cross References
- 11Composition
- 39Mechanical Properties
- 22Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 9Joints
- -Coatings
- 8Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers