PROPRIETARY Uddeholm Idun Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2018-07
Total number of updates: 2
Update History
2018-06

This material has 44 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Idun Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.21
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
13.5
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.45
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Böhler-Uddeholm AG, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Idun Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 44 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Idun Heat Treatments


  • It is intended for use in the as-delivered condition, i.e. hardened and tempered to 42–46 HRC. When the steel is to be heat treated to a higher hardness, instructions below are to be followed.
    Soft annealing: Protect the steel and heat through to 780°C (1430°F). Cool at 28°C (50°F) per hour to 600°C (1110°F), then cool freely in air.
    Stress relieving: After rough machining, the component should be heated through to max. 500°C (930°F), holding time 2 hours, then cool freely in air.
    Hardening: It is recommended to do soft annealing before hardening. Preheating temperature: 500–600°C (930–1110°F). Austenitizing temperature: 980–1000°C (1800– 1830°F) but usually 980°C (1800°F). The steel should be heated through to the austenitizing temperature and held at temperature for 30 minutes. Protect the component against decarburization and oxidation during the hardening process.
    Quenching media: Vacuum with sufficient positive pressure; High speed gas/circulating atmosphere. In order to obtain the optimum properties, the cooling rate should be as fast as possible within acceptable distortion limits. Temper the component as soon as its temperature reaches 50–70°C (120–160°F).
    Tempering: Choose the tempering temperature according to the hardness required by reference to the tempering graph. Temper minimum twice with intermediate cooling to room temperature. Lowest tempering temperature 250°C (480°F). Holding time at temperature minimum 2 hours.

PROPRIETARY Uddeholm Idun Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1490 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
12 %
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

PROPRIETARY Uddeholm Idun International Equivalent Materials


Showing 1 of 2 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Composition 100%

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 2 international equivalents?

See all 2 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 2Cross References

  • 7Composition
  • 17Mechanical Properties
  • 12Physical Properties
  • 2Heat Treatment
  • -Metallography
  • -Machinability

  • 2Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 2Total Suppliers