MPIF MIM-420 Stainless steels
Data updates
This material has 57 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
MPIF MIM-420 Chemical Composition
MPIF Standard 35 - MIM: 2025 / Materials Standard for Metal Injection Molded Parts
Looking for full material performance data?
Free registration required • Instant access
MPIF MIM-420 Physical Properties
Temperature
This material has 57 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
MPIF MIM-420 Heat Treatments
- HIP processing parameters: 1120°C (2050°F) 103 MPa (15,000 psi) for 4 hours
Heat-treated parts were austenitized and tempered at 204°C (400°F) for a minimum of 1 hour.
MPIF MIM-420 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
MPIF MIM-420 International Equivalent Materials
Showing 15 of 23 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 23 international equivalents?
See all 23 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 23Cross References
- 6Composition
- 14Mechanical Properties
- 9Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 3Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers