AIR XC 65 Structural and constructional steels
Data updates
This material has 44 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AIR XC 65 Chemical Composition
AIR 9160/C: 1973 / General conditions for delivery and use of wrought steels used in aeronautical structures
Looking for full material performance data?
Free registration required • Instant access
AIR XC 65 Physical Properties
Temperature
This material has 44 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AIR XC 65 Heat Treatments
- Hardened and tempered (T1000): Hardened at 800 +/- 10°C, Tempered at 550 +/- 5°C;
Annealed (R) at 810-835°C, cooled in calm air;
Hardened and tempered (T1000, T900 and T800): Hardened at 790 - 810°C, Tempered at min. 550°C.
AIR XC 65 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AIR XC 65 International Equivalent Materials
Showing 1 of 11 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 11 international equivalents?
See all 11 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 11Cross References
- 5Composition
- 24Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers