PROPRIETARY UHB 15N20 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2017-10
Total number of updates: 1
Update History

This material has 34 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY UHB 15N20 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.75
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.11
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.40
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

Böhler-Uddeholm AG, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY UHB 15N20 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Thermal Conductivity
49 W/(m∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 34 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY UHB 15N20 Heat Treatments


  • Hardened at 800°C and tempered for 30 minutes at temperatures given in mechanical properties.

PROPRIETARY UHB 15N20 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
620 — 1520 MPa
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
32 — 65
Unlock full details
Full data available with free access View Complete Material Data
Vickers Hardness (HV)
320 — 820
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 7Composition
  • 14Mechanical Properties
  • 10Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • 1Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers