1.4955 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2016-10
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Yield Strength, Rp0.2 460 MPa view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 600 — 750 MPa view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 66.7 ksi view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 87 — 108.8 ksi view details
Elongation, A 15 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Density 7.77 kg/dm³ view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 25.7 — 26.4 W/(m∙°C) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Heat Capacity 456 J/(kg∙°C) view details
Density 0.281 lb/in³ view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 14.8 — 15.3 BTU/(h∙ft∙°F) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Heat Capacity 0.109 BTU/(lb∙°F) view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
≤ 0.02
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
C
VALUE
0.10 – 0.14
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
8.00 – 9.50
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Nb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2

EN 10213: 2007 / Steel castings for pressure purposes

Heat Treatments