VdTÜV P 460/630 Structural and constructional steels
Data updates
This material has 24 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
VdTÜV P 460/630 Chemical Composition
WB 531: 2017 / High-strength, alloyed fine grained steel 460/630 for operating temperatures up to -40°C, sheet, hot pressed bottoms
Looking for full material performance data?
Free registration required • Instant access
VdTÜV P 460/630 Physical Properties
Temperature
This material has 24 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
VdTÜV P 460/630 Heat Treatments
- The stress relief annealing is usually carried out in the temperature range 530-560°C with a holding time of 60 minutes. If annealed at higher temperatures, the maximum holding period should be limited to 30 minutes.
VdTÜV P 460/630 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
VdTÜV P 460/630 International Equivalent Materials
Showing 2 of 2 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 2 international equivalents?
See all 2 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 2Cross References
- 13Composition
- 5Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers