VdTÜV LStE 355 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country / Standard: Germany / VdTÜV
Indicative price:

Data updates

Latest Update: 2016-02
Total number of updates: 1
Update History

This material has 55 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV LStE 355 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
≥ 0.030
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
C
VALUE
0.20 – 0.24
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
1.00 – 1.50
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

WB 461: 2001 / Fine grained steel with resistance to intergranular stress corrosion cracking with a minimum yield strength of 355 N/mm², material No.1.0569

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV LStE 355 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 55 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV LStE 355 Heat Treatments


  • Normalized: 890 to 930°C, after reaching the temperature in the entire cross-section, cooling in still air; Tempered: at 750°C (Stress realived: 580 to 620°C), at 780°C (Stress relieved: 750 to 780°C), 30 to 90 min cooling in still air (for wt <= 15mm holding time is >=15min and for 15 < wt <= 30mm holding time is >=30min).

VdTÜV LStE 355 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
490 — 650 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 6Composition
  • 44Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers