PROPRIETARY S35CK Structural and constructional steels
Material group:
Ferrous Alloys / Structural and constructional steels
Country / Standard:
PROPRIETARY
Indicative price:
Data updates
Latest Update: 2016-01
Total number of updates: 2
Update History
2015-12
This material has 12 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY S35CK Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.3200
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.7500
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
0.0180
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
Databook on fatigue strength of metallic materials, chairman: Kazuaki Shiozawa, JSMS, The Society of Materials Science, Japan and Elsevier, 1996
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY S35CK Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.67 — 7.86
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 12 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY S35CK Heat Treatments
- Heat treatment 1: Heat treated at 870°C for 1h, oil cooled. Post heat treated at 180°C for 1h, furnace cooled. Heat treatment 2: Heat treated at 920°C for 3.8h, furnace cooled, then heat treated at 900°C for 0.7h, oil cooled. Post heat treated at 180°C for 1h, furnace cooled.
Optimize material selection for your application - Book A Demo
- -Cross References
- 5Composition
- -Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 3Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers