AFCEN X5 CrNiCuNb 17-4 Stainless steels
Data updates
This material has 20 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFCEN X5 CrNiCuNb 17-4 Chemical Composition
M 3206: RCC-M II: 2024 / Martensitic stainless steel rolled or forged bars for use in manufacturing class 2 and 3 control valve blanks or cages
Looking for full material performance data?
Free registration required • Instant access
AFCEN X5 CrNiCuNb 17-4 Physical Properties
Temperature
This material has 20 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFCEN X5 CrNiCuNb 17-4 Heat Treatments
- Bars shall be delivered in the as-treated condition.
Heat treatment for mechanical properties, shall consist of the following operations:
- austenitizing at a temperature between 1020°C and 1060°C, followed by cooling in air, oil, or water + polymer down to a temperature lower or equal to 30°C,
- hardening treatment at a temperature of 480°C ± 10°C for at least 1 hour, followed by air cooling.
AFCEN X5 CrNiCuNb 17-4 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 2Cross References
- 9Composition
- 4Mechanical Properties
- 4Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers