PROPRIETARY X 260W HTM Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2015-10
Total number of updates: 1
Update History

This material has 11 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY X 260W HTM Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
2.7600
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
26.0000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
1.1200
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-33-7

Sintec HTM AG, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY X 260W HTM Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.61 — 8.1 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 11 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY X 260W HTM Heat Treatments


  • Soft annealed to 900 - 920°C, 2h. Stress-relieve annealed at 590 - 640°C, 2h, furnace cooled down to 600°C, followed by cooling in still air or furnace. Slow heating to hardening temperature of 1080 - 1180°C, 10 - 30min.

PROPRIETARY X 260W HTM Mechanical Properties


Temperature

PROPERTY / VALUE
Rockwell Hardness (HR)
56
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 5Composition
  • 1Mechanical Properties
  • 3Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers