PROPRIETARY X 235 HTM Stainless steels
Material group:
Ferrous Alloys / Stainless steels
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2015-10
Total number of updates: 1
Update History
This material has 19 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY X 235 HTM Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
2.3000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
20.0000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
1.0000
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Nb+Ta
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
Sintec HTM AG, Product Data Sheets,
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY X 235 HTM Physical Properties
Temperature
Modulus of Elasticity
190 — 218
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
14
W/(m∙°C)
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.55 — 8.1
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
This material has 19 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY X 235 HTM Heat Treatments
- Normalised up to 900 - 920°C, 2h. Hardened 1010 - 1110°C, 10 - 30 min, cooled in either air, gas, hot bath or with oil. Stress-relieve annealed at 590 - 640°C for 2h, cooled in furnace. Heat treatment 1: hardened at 1050°C. Tempered at 460°C. Heat treatment 2: hardened at 1110°C. Tempered at 450°C. Heat treatment 2: hardened at 1080°C. Tempered at 500°C.
PROPRIETARY X 235 HTM Mechanical Properties
Temperature
Tensile Strength
1591
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Compression Strength
3680
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Rockwell Hardness (HR)
59 — 64
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 6Composition
- 5Mechanical Properties
- 6Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers