AFNOR NF GX160CrMoV12 Cast steels

Material group: Ferrous Alloys / Cast steels
Country / Standard: France / AFNOR NF

Data updates

Latest Update: 2020-12
Total number of updates: 2
Update History
2015-09

This material has 12 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

AFNOR NF GX160CrMoV12 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.50 – 1.70
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
11 – 13
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.3 – 1.0
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-33-7

NF A 32-058: 2019 / Foundry products - Abrasion resistant cast steels

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

AFNOR NF GX160CrMoV12 Heat Treatments


  • Quenched and tempered (+QT1): Air or oil quenched at 980 to 1030°C. Quenched normally preceded by a full annealing treatment. Quenching:
    still air, for t ≤ 100mm,
    supply air, for t ≤ 140 mm
    oil, for t ≤ 280 mm.
    Tempered at 150 to 260°C
    Quenched and tempered (+QT2): Air or oil quenched at 980 to 1030°C. Quenched normally preceded by a full annealing treatment. Quenching:
    still air, for t ≤ 100mm,
    supply air, for t ≤ 140 mm
    oil, for t ≤ 280 mm.
    Tempered at 400 to 520°C + 150 to 260°C
    Structure:
    - for +QT1 condition - Martensitic, austenitic, carbide
    - for +QT2 condition - Martensitic, carbide (austenitic)
    Annealed at 700°C to 760°C or Fully annealed at 950 to 1100°C, and cooled 25°C / h up to 550°C or Fully annealed at 950 to 1100°C, and cooled isothermal bearing 760°C (4 to 10 h)

AFNOR NF GX160CrMoV12 Mechanical Properties


Temperature

PROPERTY / VALUE
Rockwell Hardness (HR)
58 — 62
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 9Composition
  • 2Mechanical Properties
  • -Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers