AFNOR NF G45Si7 Cast steels
Data updates
This material has 10 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF G45Si7 Chemical Composition
NF A 32-058: 2019 / Foundry products - Abrasion resistant cast steels
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF G45Si7 Heat Treatments
- Normalized (+N) at 880 to 920°C
Quenched and tempered (+QT): Oil or water quenched at 880 to 920°C and tempered at 230 to 650°C
Structure:
- for +N condition - Pearlitic
- for +QT condition - Bainitic and martensitic
AFNOR NF G45Si7 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF G45Si7 International Equivalent Materials
Showing 1 of 1 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1 international equivalents?
See all 1 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1Cross References
- 5Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers