PROPRIETARY CPM S35VN Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2015-08
Total number of updates: 1
Update History

This material has 17 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY CPM S35VN Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.4000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
14.0000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
2.0000
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Nb
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Crucible Industries LLC., Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY CPM S35VN Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 221 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.47 — 8.1 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 17 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY CPM S35VN Heat Treatments


  • Forged: 1150°C. Do not forge below 950°C. Annealed: Heat to 900°C, hold 2 hours, slow cool no faster than 15°C per hour to 595°C, then furnace cool or cool in still air to room temperature. Stress relieved: Annealed Parts: Heat to 595-705°C, hold 2 hours, then furnace cool or cool in still air. Hardened Parts: Heat to 15-30°C below original tempered temperature, hold 2 hours, then furnace cool or cool in still air. Straightened: Best done warm 200-425°C. Hardened: Preheat: Heat to 845-870°C Equalize. Austenitize: 1035-1095°C, hold time at temperature 15-30 minutes. Quench: Air or positive pressure quench (2 bar minimum) to below 50°C, or salt or interrupted oil quench to about 540°C, then air cool to below 50°C. Temper: Double temper at 200-400°C. Hold for 2 hours minimum each time.

PROPRIETARY CPM S35VN Mechanical Properties


Temperature

PROPERTY / VALUE
Brinell Hardness (HB)
255
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
16 J
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 5Composition
  • 2Mechanical Properties
  • 8Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers