MIM-430-210 (Germany / DIN) Material Properties

Material group: Ferrous Alloys / Stainless steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2019-05
Total number of updates: 3
Update History:
2015-06 2015-05

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 210 MPa view details
Tensile Strength 350 MPa view details
Elongation, A 20 % view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 30.5 ksi view details
Tensile Strength 50.8 ksi view details
Elongation, A 20 % view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 215 GPa view details
Density 7.5 — 8.1 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 31.2 E+03 ksi view details
Density 0.271 — 0.293 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.08
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.0 – 18.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Fe
VALUE
Balance
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN ISO 22068: 2014 / Sintered-metal injection-moulded materials - Specifications