PROPRIETARY JGH-Core 35JGH135 Magnetic and electrical materials
Material group:
Ferrous Alloys / Magnetic and electrical materials
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2023-10
Total number of updates: 3
Update History
2019-11
2015-03
This material has 44 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY JGH-Core 35JGH135 Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Resistivity
0.49
Ω∙mm²/m
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.65 — 7.8
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Conductivity
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
This material has 44 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY JGH-Core 35JGH135 Heat Treatments
- Stress-relief annealing is performed to remove such strain and to restore the inherent good magnetic properties. Stress-relief annealing may vary according to the degree of fabrication and the type of annealing equipment.
Heating and cooling rates: Magnetic properties are not affected by heating or cooling rates as performed on an ordinary industrials scale. However, care must be taken so that no strain will remain in the material.
Annealing temperature and holding time: Optimum annealing temperature range is 780 - 850°C. (1436 - 1562°F). Material must be maintained until heated up uniformly within this temperature range. Holding time varies depending upon the shape of core, the number of coils charged and the type of furnace.
PROPRIETARY JGH-Core 35JGH135 Mechanical Properties
Temperature
Tensile Strength
348 — 408
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
8 — 32
%
Unlock full details
Full data available with free access
View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
330 — 344
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- -Composition
- 32Mechanical Properties
- 10Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers