NMX B-181 Grade P11 Structural and constructional steels
Data updates
This material has 40 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
NMX B-181 Grade P11 Chemical Composition
NMX-B-181: 1988 / Seamless ferritic alloy-steel pipe for high temperature service
Looking for full material performance data?
Free registration required • Instant access
NMX B-181 Grade P11 Physical Properties
Temperature
This material has 40 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
NMX B-181 Grade P11 Heat Treatments
- If furnished in the normalized and tempered condition, the minimum tempering temperature shall be 650°C. It is recommended that the temperature for tempering should be at least 50°C above the intended service temperature; consequently, the purchaser should advise the manufacturer if the service temperature is to be over 600°C.
NMX B-181 Grade P11 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 23Cross References
- 7Composition
- 6Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers