PROPRIETARY 40CrNi2Si2MoVA Structural and constructional steels
Data updates
This material has 70 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY 40CrNi2Si2MoVA Chemical Composition
China Aeronautical Materials Handbook, 2001
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY 40CrNi2Si2MoVA Physical Properties
Temperature
This material has 70 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY 40CrNi2Si2MoVA Heat Treatments
- Heat treatment 1: Quenched at 870°C, oil. Tempered twice at 300°C, air cooled. Heat treatment 2: Heat treated at 870°C. Austempered at 270°C. Tempered twice at 300°C, air cooled.
PROPRIETARY 40CrNi2Si2MoVA Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY 40CrNi2Si2MoVA International Equivalent Materials
Showing 2 of 6 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 6 international equivalents?
See all 6 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 6Cross References
- 10Composition
- 14Mechanical Properties
- 12Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 25Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers