MIL S-15464B Class 1 Cast steels

Material group: Ferrous Alloys / Cast steels
Country / Standard: United States / MIL

Data updates

Latest Update: 2014-10
Total number of updates: 1
Update History

This material has 16 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

MIL S-15464B Class 1 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.2000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.0000 – 1.5000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.5000
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

MIL-S-15464B: 1953 / Steel alloy, chromium-molybdenum; castings

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

MIL S-15464B Class 1 Heat Treatments


  • Annealing: heated to 10-65°C (50-150°F) above the upper critical point, cooled in the furnace to 399°C (750°F), after which the cooling rate of the furnace may be accelerated. When the temperature of the hottest part of the charge has fallen to 260°C (500°F), the castings may be removed from the furnace and cooled in still air; Normalizing: heated to and held at a temperature of at least 38°C (100°F) above the upper critical point. Castings shall then be removed from the furnace and permitted to cool through the critical range in air; Tempering: heating uniformly at a controlled rate to 593-704°C (1100-1300°F). Mechanical properties of normalized or quenched castings shall be determined after tempering; Stress relief heat treatment - shall be at least 16°C (60°F) but not more than 38°C (100°F) below the tempering temperature; Homogenization: heated to 1010 to 1288°C (1850 to 2350°F) and shall be held at the homogenization temperature a sufficient length of time to minimize harmful heterogeneity by diffusion. The castings shall then be withdrawn to cool through the critical range.

MIL S-15464B Class 1 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 483 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 20 %
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
≥ 276 MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 2Cross References

  • 9Composition
  • 4Mechanical Properties
  • -Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers