PROPRIETARY PV6 Tool steels
Data updates
This material has 300 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY PV6 Chemical Composition
Dörrenberg Edelstahl GmbH, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY PV6 Physical Properties
Temperature
This material has 300 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY PV6 Heat Treatments
- Soft annealing: 720 - 750°C, furnace cooling.
Stress Relieving: 600 - 650°C, furnace cooling.
Hardening: 830 - 870°C, oil or hot bath 180 - 220°C cooling. - Soft annealed: 720-750°C, furnace cooled (HB ≤ 223)
Stress relief annealed: 600-650°C, furnace cooled
Hardened: 830-870°C, oil cooled or hot bath 180-220°C
PROPRIETARY PV6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY PV6 International Equivalent Materials
Showing 15 of 148 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 148 international equivalents?
See all 148 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 148Cross References
- 4Composition
- 3Mechanical Properties
- 17Physical Properties
- 5Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 123Total Suppliers