PROPRIETARY Thermodur 2367 Superclean Tool steels
Material group:
Ferrous Alloys / Tool steels
Country / Standard:
PROPRIETARY
Data updates
Latest Update: -
Total number of updates: 0
This material has 13 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Thermodur 2367 Superclean Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.3700
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
5.0000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
3.0000
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
Schmolz + Bickenbach, Product Data Sheets,
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Thermodur 2367 Superclean Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.72 — 8
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 13 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Thermodur 2367 Superclean Heat Treatments
- Soft annealing: 730-780°C, cooling: furnace 7°C/hour to 649°C then air cool. Stress relieving: 649°C for 2 hours, cooling: slowly to 482°C in air. Hardening: 1024-1049°C hold at temperature for 30 minutes, cooling: vacuum quench at 10°C/min. to 538°C then cool to below 65°C.
PROPRIETARY Thermodur 2367 Superclean Mechanical Properties
Temperature
Brinell Hardness (HB)
≤ 235
Unlock full details
Full data available with free access
View Complete Material Data
Rockwell Hardness (HR)
≤ 55
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 6Composition
- 2Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers