SA-268 S44627 (United States / ASME) Material Properties
Alternative designations:
27Cr-1Mo
Material group:
Ferrous Alloys / Stainless steels
Country/Standard:
United States / ASME
Data updates
Latest Update: 2024-02
Total number of updates: 7
Update History:
2023-11
2023-10
2022-04
2020-10
2016-02
2016-01
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.01
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
25.0 – 27.5
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.2
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Nb
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
ASME Boiler and Pressure Vessel Code An International Code Section II - Part A Ferrous Material Specifications / American Society of Mechanical Engineers / 2023
Heat Treatments
- As a final heat treatment, tubes shall be reheated to a temperature of 650°C (1200°F) or higher and cooled.
-
25 Cross References
-
11 Composition
-
40 Mechanical Properties
-
5 Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
30 Creep
-
- Joints
-
- Coatings
-
55 Dimensions
-
- Tribology
-
4588 Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
5 Total Suppliers