ISO 20MnB4 Structural and constructional steels
Data updates
This material has 395 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ISO 20MnB4 Chemical Composition
ISO/TR 11637: 1997 / Boron treated engineering steels for quenching and tempering
Looking for full material performance data?
Free registration required • Instant access
ISO 20MnB4 Physical Properties
Temperature
This material has 395 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ISO 20MnB4 Heat Treatments
- Core hardened (+CH): Austenitizing temperature in the core hardening test at 880°C (± 5°C), a hardening time at temperature of at least 30 min is recommended.
ISO 20MnB4 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ISO 20MnB4 International Equivalent Materials
Showing 15 of 145 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 145 international equivalents?
See all 145 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 145Cross References
- 27Composition
- 41Mechanical Properties
- 3Physical Properties
- 4Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 45Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 130Total Suppliers