EN-GJS-SiMo40-6 (European Union / EN) Material Properties

Other designations:
Material group: Ferrous Alloys / Cast irons
Country/Standard: European Union / EN

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 480 MPa view details
Elongation, A 8 % view details
Brinell Hardness (HB) 190 — 240 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 69.6 ksi view details
Elongation, A 8 % view details
Brinell Hardness (HB) 190 — 240 view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Mo
VALUE
0.5 – 0.7
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Si
VALUE
3.8 – 4.2
UNIT
%
CAS NUMBER
7440-21-3

EN 16124: 2011 / Founding - Low-alloyed ferritic spheroidal graphite cast irons for elevated temperature applications