GB BTMCr26 Cast irons
Data updates
This material has 25 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
GB BTMCr26 Chemical Composition
GB/T 8263: 2025 / Abrasion-resistant white iron castings
Looking for full material performance data?
Free registration required • Instant access
GB BTMCr26 Heat Treatments
- Soft annealed at 960-1060°C, hold at that temperature. Slowly cooled at 680-750°C, hold at that temperature. Slowly cooled to below 600°C, air or furnace cooled.
Hardened at 950-1050°C, rapidly cooled.
Tempered at 200-550°C, air or furnace cooled.
GB BTMCr26 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
GB BTMCr26 International Equivalent Materials
Showing 4 of 5 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 5 international equivalents?
See all 5 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 5Cross References
- 9Composition
- 6Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 4Total Suppliers