GB ZG15Cr13 Cast steels
Data updates
This material has 92 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
GB ZG15Cr13 Chemical Composition
JB/T 6405: 2006 / Heavy stainless steel castings
Looking for full material performance data?
Free registration required • Instant access
GB ZG15Cr13 Heat Treatments
- Heated to 950 °C - 1050 °C, thermal insulated, air cooling; and at 650 °C - 750 °C, tempering, air cooling
- Quenching (or Normalizing) Temperature: minimum 950°C
Tempering Temperature: 680°C – 740°C
Stress Relief Annealing Temperature: minimum 650°C
GB ZG15Cr13 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
GB ZG15Cr13 International Equivalent Materials
Showing 15 of 46 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 46 international equivalents?
See all 46 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 46Cross References
- 25Composition
- 14Mechanical Properties
- -Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers