MSZ NCMo V Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country / Standard: Hungary / MSZ

Data updates

Latest Update: 2017-07
Total number of updates: 1
Update History

This material has 36 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

MSZ NCMo V Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.3300 – 0.4000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.2000 – 1.5000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.2500 – 0.5000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

MSZ 61: 1985 / Heat-treatable steels

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

MSZ NCMo V Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 36 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

MSZ NCMo V Heat Treatments


  • Quenched at 810 to 840°C in oil, min. 30 minutes.
    Tempered at 540 to 650°C, at least 1 hour.
    Softened at 620 to 650°C.
    Hot formed at 1050 to 850°C.

MSZ NCMo V Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1000 — 1450 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
≤ 285
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 9 %
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 1Cross References

  • 9Composition
  • 21Mechanical Properties
  • 3Physical Properties
  • 2Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers