MSZ KO 36Ti Stainless steels
Data updates
This material has 566 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
MSZ KO 36Ti Chemical Composition
MSZ 4360: 1987 / Stainless steel
Looking for full material performance data?
Free registration required • Instant access
MSZ KO 36Ti Physical Properties
Temperature
This material has 566 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
MSZ KO 36Ti Heat Treatments
- Hot formed at 1150 to 850°C, cooled in air.
Austenitic heat treatment (solvent, heat treatment) at 1050 to 1100°C, cooled in water or air.
MSZ KO 36Ti Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
MSZ KO 36Ti International Equivalent Materials
Showing 15 of 320 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 320 international equivalents?
See all 320 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 320Cross References
- 9Composition
- 4Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 229Total Suppliers