CSN EN-JL3011 Chemical Composition
EN 13835: 2012 / Founding - Austenitic cast irons
Looking for full material performance data?
Free registration required • Instant access
CSN EN-JL3011 Physical Properties
Temperature
This material has 190 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
CSN EN-JL3011 Heat Treatments
- Stress relieving: heat up to between 625-650°C at a rate not exceeding 150°C/h, hold within this range for 2 h plus 1 h per 25 mm section thickness, cool down to 200°C in the furnace at a rate not exceeding 100°C/h, air cool.
CSN EN-JL3011 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
CSN EN-JL3011 International Equivalent Materials
Showing 15 of 90 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 90 international equivalents?
See all 90 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 90Cross References
- 7Composition
- 9Mechanical Properties
- 17Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 66Total Suppliers