PROPRIETARY Uddeholm Viking Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2016-04
Total number of updates: 1
Update History

This material has 52 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Viking Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.5
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
8.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.5
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Uddeholms AB, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Viking Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Thermal Conductivity
val1
Full data available with free access View Complete Material Data
W/(m∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 52 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Viking Heat Treatments


  • Soft Annealing
    Protect the steel and heat through to 880°C (1620°F). Then cool in the furnace at approx. 10°C (20°F) per hour to 650°C (1200°F), then freely in air.
    Stress Relieving
    After rough machining the tool should be heated through to 650°C (1200°F), holding time 2 hours. Cool slowly to 500°C (930°F), then freely in air.
    Hardening
    Pre-heating temperature: 600 - 700°C (1110 - 1290°F). Austenitizing temperature: 980 - 1050°C (1800 - 1920°F) normally 1010°C (1850°F).
    Protection Against Decarburization
    Protection against decarburization and oxidation, while heating for hardening, is obtained by: heating in neutral salt bath, packing in spent cast-iron chips, spent coke or paper, protective atmosphere - endothermic gas, vacuum
    Quenching Media
    Circulating air or atmosphere, air blast, martempering bath 200 - 550°C (390 - 1020°F) 1 - 120 minutes, then cool in air, oil.
    Temper the tool as soon as its temperature reaches 50 - 70°C (120 - 160°F).
    Tempering
    Heating to tempering temperature should be carried out slowly and uniformly. Tempering should be carried out twice. Lowest temperature 180°C (360°F). Holding time at temperature minimum 2 hours.
    Flame And Induction Hardening
    Both flame and induction hardening methods can be applied. In order to get a very uniform hardness after flame or induction hardening the steel can first be prehardened to approx. 35 ± 2 HRC. After flame or induction hardening the steel should be tempered at at least 180°C (360°F).
  • Austenitizing temperature 1010°C (1850°F).

PROPRIETARY Uddeholm Viking Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1620 — 1960 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
≤ 225
Unlock full details
Full data available with free access View Complete Material Data
Compression Strength
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
6 — 8 %
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Compression Yield Strength
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 1Cross References

  • 6Composition
  • 22Mechanical Properties
  • 15Physical Properties
  • 3Heat Treatment
  • -Metallography
  • -Machinability

  • 3Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 2Total Suppliers