PROPRIETARY Uddeholm Ramax HH Stainless steels

Material group: Ferrous Alloys / Stainless steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2016-04
Total number of updates: 1
Update History

This material has 36 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Ramax HH Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.12
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
13.4
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
1.3
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Uddeholms AB, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Ramax HH Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 215 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 36 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Ramax HH Heat Treatments


  • Soft annealing: Protect the steel and heat through to 740°C (1365°F). Cool at 17°C (30°F) per hour to 550°C (1020°F), then freely in air;
    Stress relieving: After rough machining the tool should be heated through to max. 530°C (985°F), holding time 2 hours, then cool freely in air;
    Hardening: (The steel should be annealed before hardening.) Preheating temperature: 500–600°C (930–1110°F). Austenitizing temperature: 980-1020°C (1795-1870°F). The steel should be heated through to the austenitizing temperature and held at temperature for 30 minutes. (Protect the tool against decarburization and oxidation during the hardening process.);
    Quenching media: Oil, Fluidized bed or salt bath at 250-550°C (480–1020°F), then cool in air blast, Vacuum with sufficient positive pressure, High speed gas/circulating atmosphere. In order to obtain the optimum properties, the cooling rate should be as fast is possible within acceptable distortion limits. Temper the tool as soon as its temperature reaches 50-70°C (120-160°F);
    Tempering: Choose the tempering temperature according to the hardness. Temper twice with intermediate cooling to room temperature. Lowest tempering temperature 250°C (480°F). Holding time at temperature minimum 2 hours. Austenitizing temperature: 1000°C (1830°F), 30 min. Holding time: 2 + 2h.

PROPRIETARY Uddeholm Ramax HH Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
1140 MPa
Unlock full details
Full data available with free access View Complete Material Data
Brinell Hardness (HB)
320 — 350
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 9Composition
  • 10Mechanical Properties
  • 9Physical Properties
  • 2Heat Treatment
  • -Metallography
  • -Machinability

  • 2Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 4Total Suppliers