PROPRIETARY F65 Structural and constructional steels
Data updates
This material has 436 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY F65 Chemical Composition
Aubert & Duval, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY F65 Physical Properties
Temperature
This material has 436 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY F65 Heat Treatments
- Annealed condition: Heat to 825°C followed by slow cooling.
Quenched and tempered (I): Oil quench from 850°C. Temper at 600°C.
Quenched and tempered (II): Oil quench from 850°C. Temper at 675°C.
Harden: Heat to 850°C; Oil quench.
Temper Depending on properties required.
Forged: 1100/900°C.
PROPRIETARY F65 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY F65 International Equivalent Materials
Showing 15 of 237 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 237 international equivalents?
See all 237 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 237Cross References
- 3Composition
- 33Mechanical Properties
- 6Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 156Total Suppliers