PN 40rs Structural and constructional steels
Data updates
This material has 381 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PN 40rs Chemical Composition
PN-H-84019: 1993 / Unalloyed wrought steel for case hardening and for quenching and tempering - Grades
Looking for full material performance data?
Free registration required • Instant access
PN 40rs Physical Properties
Temperature
This material has 381 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PN 40rs Heat Treatments
- Wrought steel: Heated at 1100-850°C, softened at 650-700°C and normalized at 850-890°C. Hardened at 830-870°C, center zone cooled in water or oil, than tempered at 550-660°C. These face of test sample hardened in the range of 870°C+/-5.
PN 40rs Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PN 40rs International Equivalent Materials
Showing 15 of 157 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 157 international equivalents?
See all 157 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 157Cross References
- 20Composition
- 68Mechanical Properties
- 3Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 131Total Suppliers