DIN HS6-5-3 Tool steels

Material group: Ferrous Alloys / Tool steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2023-10
Total number of updates: 2
Update History
2018-09

This material has 290 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN HS6-5-3 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.15 – 1.25
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
3.8 – 4.5
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-33-7

EN ISO 4957: 2018 / Tool steels

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN HS6-5-3 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 290 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN HS6-5-3 Heat Treatments

  • Austenitized at 1200 ± 10°C and quenched. Usual quenching media in practice are air, gas or salt bath. Total heating time of test pieces in a salt bath is 3 min. for hardening and minimum 2 periods of 60 min. each for tempering.
    Tempered at 560 ± 10°C.

DIN HS6-5-3 Mechanical Properties


Temperature

PROPERTY / VALUE
Brinell Hardness (HB)
≤ 269
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
48
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 131 Cross References

  • 9 Composition
  • 13 Mechanical Properties
  • 3 Physical Properties
  • 11 Heat Treatment
  • 1 Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • - Creep

  • - Joints
  • - Coatings
  • 6 Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 116 Total Suppliers