ACI CB6 Cast steels
Data updates
This material has 24 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ACI CB6 Chemical Composition
Castings Stainless Steel and Nickel base, Nickel Institute, 2012
Looking for full material performance data?
Free registration required • Instant access
ACI CB6 Heat Treatments
- Heat treated: at 980-1050°C (1800-1920°F), forced air cool to 50°C (120°F), temper 595-625°C (1100-1160°F).
ACI CB6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ACI CB6 International Equivalent Materials
Showing 7 of 7 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 7 international equivalents?
See all 7 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 7Cross References
- 8Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers