ACI CH8 Cast steels
Data updates
This material has 22 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ACI CH8 Chemical Composition
Castings Stainless Steel and Nickel base, Nickel Institute, 2012
Looking for full material performance data?
Free registration required • Instant access
ACI CH8 Heat Treatments
- Heat to 1093°C (2000°F) minimum, hold for sufficient time to heat casting uniformly to temperature, quench in water or rapid cool by other means.
ACI CH8 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ACI CH8 International Equivalent Materials
Showing 7 of 10 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 10 international equivalents?
See all 10 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 10Cross References
- 7Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers