ACI CD3MCuN Cast steels
Data updates
This material has 25 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ACI CD3MCuN Chemical Composition
Steel Castings Handbook Supplement 8 High Alloy Data Sheets Corrosion Series, Steel Founders' Society of America, 2004
Looking for full material performance data?
Free registration required • Instant access
ACI CD3MCuN Heat Treatments
- Heat to 1040°C (1900°F) minimum, hold for sufficient time to heat casting uniformly to temperature, quench in water or rapid cool by other means.
ACI CD3MCuN Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ACI CD3MCuN International Equivalent Materials
Showing 7 of 7 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 7 international equivalents?
See all 7 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 7Cross References
- 11Composition
- 3Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 3Total Suppliers